<?xml version="1.0" encoding="UTF-8"?>
<OAI-PMH xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/ http://www.openarchives.org/OAI/2.0/OAI-PMH.xsd">
  <responseDate>2026-11-24T14:08:12Z</responseDate>
  <request verb="GetRecord" identifier="oai:lifeofresearch.com:273" metadataPrefix="oai_datacite">https://lifeofresearch.com/oai2</request>
  <GetRecord>
    <record>
      <header>
        <identifier>oai:lifeofresearch.com:273</identifier>
        <datestamp>2026-11-24T12:07:12Z</datestamp>
        <setSpec>type:article</setSpec>
        <setSpec>openaire</setSpec>
      </header>
      <metadata>
        <resource xmlns="http://datacite.org/schema/kernel-4" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://datacite.org/schema/kernel-4 http://schema.datacite.org/meta/kernel-4.4/metadata.xsd">
          <identifier identifierType="URL">https://lifeofresearch.com/articles/273</identifier>
          <creators>
            <creator>
              <creatorName>KULDOSHOV SH.M.</creatorName>
              <affiliation>Institute of General and Inorganic Chemistry, Academy of Sciences of the Republic of Uzbekistan, Tashkent, Uzbekistan.</affiliation>
            </creator>
            <creator>
              <creatorName>ADINAEV KH.F.</creatorName>
              <affiliation>Institute of General and Inorganic Chemistry, Academy of Sciences of the Republic of Uzbekistan, Tashkent, Uzbekistan.</affiliation>
            </creator>
            <creator>
              <creatorName>SOATBOYEVA M.O.</creatorName>
              <affiliation>Institute of General and Inorganic Chemistry, Academy of Sciences of the Republic of Uzbekistan, Tashkent, Uzbekistan.</affiliation>
            </creator>
            <creator>
              <creatorName>RASULOVA S.N.</creatorName>
              <affiliation>Institute of General and Inorganic Chemistry, Academy of Sciences of the Republic of Uzbekistan, Tashkent, Uzbekistan.</affiliation>
            </creator>
            <creator>
              <creatorName>YULDASHEV SH.U.</creatorName>
              <affiliation>Institute of General and Inorganic Chemistry, Academy of Sciences of Uzbekistan</affiliation>
            </creator>
            <creator>
              <creatorName>ERKINBOYEVA SH.S.</creatorName>
              <affiliation>Institute of General and Inorganic Chemistry, Academy of Sciences of the Republic of Uzbekistan, Tashkent, Uzbekistan.</affiliation>
            </creator>
          </creators>
          <titles><title>HYDROMETALLURGICAL RECOVERY OF GOLD FROM ROASTED PYRITE CONCENTRATE USING A THIOUREA SYSTEM</title></titles>
          <publisher>Life of Research</publisher>
          <publicationYear>2026</publicationYear>
          <subjects>
            <subject>pyrite concentrate</subject>
            <subject>gold recovery</subject>
            <subject>thiourea</subject>
            <subject>FeCl₃</subject>
            <subject>cyanide-free leaching</subject>
            <subject>thermal activation</subject>
            <subject>hydrometallurgy</subject>
            <subject>ICP-OES.</subject>
          </subjects>
          <resourceType resourceTypeGeneral="JournalArticle">Journal article</resourceType>
          <rightsList><rights rightsURI="https://creativecommons.org/licenses/by/4.0/">Creative Commons Attribution 4.0</rights></rightsList>
          <descriptions><description descriptionType="Abstract">Background. Gold extraction from refractory sulfide materials is challenging because gold is encapsulated within pyrite, limiting the accessibility of gold-bearing components to leaching reagents. Therefore, the development of cyanide-free hydrometallurgical systems based on thiourea is relevant due to their potential for rapid gold dissolution and environmental benefits.

Purpose. To investigate gold extraction from thermally activated pyrite concentrate using an acidic FeCl₃-thiourea leaching system and evaluate the effects of thiourea concentration, temperature, and leaching time on gold dissolution.

Methodology. The experimental procedure involved grinding and granulating pyrite concentrate, thermal activation at 400–700 °C, and subsequent hydrometallurgical leaching. The concentrate calcined at 600 °C was selected for further investigation. Leaching was performed using thiourea solutions with concentrations of 0.2 and 0.3 mol/L at a solid-to-liquid ratio of 1:4. FeCl₃ was used as an oxidant, and the pH was maintained at 1.5 using HCl. Experiments were conducted at 25±2, 35, and 45 °C for 8–16 h with continuous stirring at 600 rpm. The initial and calcined samples were analyzed by scanning electron microscopy (SEM), while the gold concentration in the leaching solutions was determined by inductively coupled plasma optical emission spectrometry (ICP-OES).
Scientific novelty. The effects of thiourea concentration, temperature, and leaching time on gold dissolution from pyrite concentrate calcined at 600 °C in the FeCl₃-thiourea system were systematically investigated. Attention was given to the role of the Fe³⁺/Fe²⁺ redox couple in gold oxidation and the formation of soluble gold complexes.
Results. Thermal activation promotes oxidation of the sulfide matrix, sulfur removal, iron oxide formation, and pore development, thereby improving the accessibility of gold-bearing sites to the leaching solution. In the FeCl₃-thiourea system, gold is oxidized and stabilized in solution as soluble complexes. Leaching efficiency depends on thiourea concentration, temperature, and reaction time, whereas excessively oxidative conditions may accelerate thiourea degradation. Dissolved gold was quantified by ICP-OES to evaluate process efficiency and identify favorable operating conditions.</description></descriptions>
        </resource>