Life of Research
Appearance

HYDROMETALLURGICAL RECOVERY OF GOLD FROM ROASTED PYRITE CONCENTRATE USING A THIOUREA SYSTEM

  • KULDOSHOV SH.M.1
  • ADINAEV KH.F.1
  • SOATBOYEVA M.O.1
  • RASULOVA S.N.1
  • YULDASHEV SH.U.2
  • ERKINBOYEVA SH.S.1
  1. 1Institute of General and Inorganic Chemistry, Academy of Sciences of the Republic of Uzbekistan, Tashkent, Uzbekistan.
  2. 2Institute of General and Inorganic Chemistry, Academy of Sciences of Uzbekistan

Journal article

LOR-00273

Download PDF (1.7 MB) Cite

Cite

HYDROMETALLURGICAL RECOVERY OF GOLD FROM ROASTED PYRITE CONCENTRATE USING A THIOUREA SYSTEM

Read

Abstract

Background. Gold extraction from refractory sulfide materials is challenging because gold is encapsulated within pyrite, limiting the accessibility of gold-bearing components to leaching reagents. Therefore, the development of cyanide-free hydrometallurgical systems based on thiourea is relevant due to their potential for rapid gold dissolution and environmental benefits.

Purpose. To investigate gold extraction from thermally activated pyrite concentrate using an acidic FeCl₃-thiourea leaching system and evaluate the effects of thiourea concentration, temperature, and leaching time on gold dissolution.

Methodology. The experimental procedure involved grinding and granulating pyrite concentrate, thermal activation at 400–700 °C, and subsequent hydrometallurgical leaching. The concentrate calcined at 600 °C was selected for further investigation. Leaching was performed using thiourea solutions with concentrations of 0.2 and 0.3 mol/L at a solid-to-liquid ratio of 1:4. FeCl₃ was used as an oxidant, and the pH was maintained at 1.5 using HCl. Experiments were conducted at 25±2, 35, and 45 °C for 8–16 h with continuous stirring at 600 rpm. The initial and calcined samples were analyzed by scanning electron microscopy (SEM), while the gold concentration in the leaching solutions was determined by inductively coupled plasma optical emission spectrometry (ICP-OES).
Scientific novelty. The effects of thiourea concentration, temperature, and leaching time on gold dissolution from pyrite concentrate calcined at 600 °C in the FeCl₃-thiourea system were systematically investigated. Attention was given to the role of the Fe³⁺/Fe²⁺ redox couple in gold oxidation and the formation of soluble gold complexes.
Results. Thermal activation promotes oxidation of the sulfide matrix, sulfur removal, iron oxide formation, and pore development, thereby improving the accessibility of gold-bearing sites to the leaching solution. In the FeCl₃-thiourea system, gold is oxidized and stabilized in solution as soluble complexes. Leaching efficiency depends on thiourea concentration, temperature, and reaction time, whereas excessively oxidative conditions may accelerate thiourea degradation. Dissolved gold was quantified by ICP-OES to evaluate process efficiency and identify favorable operating conditions.

Keywords

Files (1)

Cite this record

SH.M., K., KH.F., A., M.O., S., S.N., R., SH.U., Y., & SH.S., E. (2026). HYDROMETALLURGICAL RECOVERY OF GOLD FROM ROASTED PYRITE CONCENTRATE USING A THIOUREA SYSTEM. Life of Research. https://lifeofresearch.com/articles/273

APA 7th edition
Export to a reference manager
BibTeX
@misc{shm2026hydrometallurgical,
  author       = {SH.M., KULDOSHOV and KH.F., ADINAEV and M.O., SOATBOYEVA and S.N., RASULOVA and SH.U., YULDASHEV and SH.S., ERKINBOYEVA},
  title        = {{HYDROMETALLURGICAL RECOVERY OF GOLD FROM ROASTED PYRITE CONCENTRATE USING A THIOUREA SYSTEM}},
  year         = {2026},
  month        = oct,
  date         = {2026-10-24},
  publisher    = {Life of Research},
  url          = {https://lifeofresearch.com/articles/273},
  abstract     = {Background. Gold extraction from refractory sulfide materials is challenging because gold is encapsulated within pyrite, limiting the accessibility of gold-bearing components to leaching reagents. Therefore, the development of cyanide-free hydrometallurgical systems based on thiourea is relevant due to their potential for rapid gold dissolution and environmental benefits.

Purpose. To investigate gold extraction from thermally activated pyrite concentrate using an acidic FeCl₃-thiourea leaching system and evaluate the effects of thiourea concentration, temperature, and leaching time on gold dissolution.

Methodology. The experimental procedure involved grinding and granulating pyrite concentrate, thermal activation at 400–700 °C, and subsequent hydrometallurgical leaching. The concentrate calcined at 600 °C was selected for further investigation. Leaching was performed using thiourea solutions with concentrations of 0.2 and 0.3 mol/L at a solid-to-liquid ratio of 1:4. FeCl₃ was used as an oxidant, and the pH was maintained at 1.5 using HCl. Experiments were conducted at 25±2, 35, and 45 °C for 8–16 h with continuous stirring at 600 rpm. The initial and calcined samples were analyzed by scanning electron microscopy (SEM), while the gold concentration in the leaching solutions was determined by inductively coupled plasma optical emission spectrometry (ICP-OES). Scientific novelty. The effects of thiourea concentration, temperature, and leaching time on gold dissolution from pyrite concentrate calcined at 600 °C in the FeCl₃-thiourea system were systematically investigated. Attention was given to the role of the Fe³⁺/Fe²⁺ redox couple in gold oxidation and the formation of soluble gold complexes. Results. Thermal activation promotes oxidation of the sulfide matrix, sulfur removal, iron oxide formation, and pore development, thereby improving the accessibility of gold-bearing sites to the leaching solution. In the FeCl₃-thiourea system, gold is oxidized and stabilized in solution as soluble complexes. Leaching efficiency depends on thiourea concentration, temperature, and reaction time, whereas excessively oxidative conditions may accelerate thiourea degradation. Dissolved gold was quantified by ICP-OES to evaluate process efficiency and identify favorable operating conditions.},
  keywords     = {pyrite concentrate, gold recovery, thiourea, FeCl₃, cyanide-free leaching, thermal activation, hydrometallurgy, ICP-OES.},
  language     = {en},
  copyright    = {Creative Commons Attribution 4.0}
}

Using Zotero or Mendeley? Their browser connector saves this record from this page, with its PDF when there is one. On search and browse pages it lists every result so you can save many at once.

Guides What a complete citation needs What CC BY 4.0 allows